MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Danquinsa DANADD® MB-51HY-POWDER Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DANADD® MB-51HY-POWDER is a special additive, supplied as powder which should act as additive resp. for the improvement of the hydrolysis resistance at TPU raw materials. This high-grade Polycarbodiimid has a slightly yellow till brownish inherent color. . DANADD® MB-51HY-POWDER can be applied and added to all PEARLTHANE® TPUs based on polyether, polyester and polycaproalcton polyester in order to achieve a betterment relating to the hydrolysis resistance.

Application: DANADD® MB-51HY-POWDER is added to the PEARLTHANE® TPUs which are used for the processing by extrusion and injection moulding. We recommend to add DANADD® MB-51HYPOWDER directly to the PEARLTHANE®-TPUs. The powder should adhere well onto the pearl granules of the PEARLTHANE® TPUs. DANADD ® MB-51HY-POWDER can be also applied via the color masterbatch dosing plants in order to add them to the nature TPU granules. We recommend additions of 0,5-1,0%. From this additive powder, calculated onto the TPU granule.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 80.0 - 180 °CKOFLER
Softening Point 90.0 °CKOFLER
Flash Point 310 °CDIN ISO 2592
Ignition Temperature 455 °CDIN 51.794
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.050 %Residual; MQSA-Nr.: 44
Shelf Life 6.00 Month
 
Descriptive Properties
Active content1MQSA-No.: 39a
AspectFine, regular, yellowish until brownish powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDANQ010 / 294430

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.