MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Radici RADISTRONG® AROMA RV500RKC2 106 NT Nylon 66//Nylon, 50% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: Description: Special PA 50% glass fibre reinforced, high flow injection moulding grade. Heat stabilized. Drinking water and food contact. Natural colour. General purpose metal replacement product with good resistance to hydrolysis, enhanced mechanical properties after moisture pick-up. Specifically intended for use in applications in civil and industrial water management as well as appliances and consumer goods. Suitable for parts requiring very high stiffness and high mechanical resistance along with high surface quality and superior gloss.

Processing: Injection Molding

Delivery Form: Granules

Additives: Release agent

Special Characteristics: Heat stabilized or stable to heat, Improved Fluiditiy, Hydrolysis Resistance, Food Contact, High Surface Aspect

Industries: Consumer Industry Goods, Water Management

Regional Availability: North America, Europe, Asia Pacific, South and Central America, Near East/Africa

Information provided by Radici Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.59 g/cc0.0574 lb/in³ISO 1183
Moisture Absorption 1.10 %
@Thickness 2.00 mm
1.10 %
@Thickness 0.0787 in
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inMelt Temp/Mold Temp/Cavity Pressure: 290/80/60; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inMelt Temp/Mold Temp/Cavity Pressure: 290/80/60; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 260 MPa37700 psi5mm/min; ISO 527-2/1A
Elongation at Break 3.2 %3.2 %5mm/min; ISO 527-2/1A
Tensile Modulus 17.9 GPa2600 ksi1mm/min; ISO 527-2/1A
Flexural Strength 400 MPa58000 psi2mm/min; ISO 178
Flexural Modulus 16.8 GPa2440 ksi2mm/min; ISO 178
Charpy Impact Unnotched 11.0 J/cm²52.3 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.70 J/cm²8.09 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 19.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
10.6 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 68.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
37.8 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
Melting Point 260 °C500 °FISO 11357-1/-3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °F
Mold Temperature 80.0 - 100 °C176 - 212 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADICI042 / 313543

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.