Product Description: Toughblend® PA66-1900 is a glass fiber reinforced compound offering high mechanical and thermal properties for high end product application. Features: - Glass Fiber Reinforcement, 45%
- High thermal properties
- High mechanical properties
- High impact strength
Uses:- Automotive Applications
- Industrial parts
Forms:Processing Method:Information provided by Colour Image Plastic Compound Sdn Bhd |