SABIC® HDPE 551010000 (black) is a grade, which has a high density (class MRS 8 - PE 80) and a bimodal distribution of the molecular mass. An universal grade for pipe extrusion which, due to a keen combination of properties, is particularly suitable for drinking water and waste water piping. It is also used for the manufacture of chemical apparatus and containers. This material meets (inter)national standards for use in drinking water and wastewater piping.Information provided by SABIC |