MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Magnesium AZ31B-O, Annealed Sheet
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: AZ31B and AZ31C have the same nominal composition and differ only in specification ranges.

Key Words: UNS M11311; Mg
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.77 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 56500 kg load, 10 mm ball
Hardness, Knoop 71Estimated from Brinell
Hardness, Vickers 83Estimated from Brinell
Tensile Strength, Ultimate 255 MPa
Tensile Strength, Yield 150 MPa
@Strain 0.2 %
Elongation at Break 21 %in 50 mm
Tensile Modulus 45.0 GPa
Compressive Yield Strength 110 MPaat 0.2% offset
Ultimate Bearing Strength 485 MPa
Bearing Yield Strength 290 MPa
Poissons Ratio 0.35
Fatigue Strength 120 - 145 MPa
@# of Cycles 1.00e+7
Axially-loaded flat specimen, R=1/4
Machinability 100 %Relative Rating, 100=Best
Shear Modulus 17.0 GPa
Shear Strength 145 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000920 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 340 J/g
CTE, linear 26.0 µm/m-°C
@Temperature 0.000 - 100 °C
 27.0 µm/m-°C
@Temperature 20.0 - 200 °C
Estimated from similar Mg alloys
Specific Heat Capacity 1.00 J/g-°C
Thermal Conductivity 96.0 W/m-K
Melting Point 605 - 630 °C
Solidus 605 °C
Liquidus 630 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 230 - 425 °CHot Working
Annealing Temperature 345 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 2.5 - 3.5 %
Calcium, Ca <= 0.040 %
Copper, Cu <= 0.050 %
Iron, Fe <= 0.0050 %
Magnesium, Mg 96 %As Remainder
Manganese, Mn >= 0.20 %
Nickel, Ni <= 0.0050 %
Silicon, Si <= 0.10 %
Zinc, Zn 0.60 - 1.4 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Magnesium AZ31B-H24, Hard Rolled Sheet
Magnesium AZ31B-F, Extruded Solid Shapes
Magnesium AZ31B-H26, Hard Rolled Sheet
Magnesium AZ31B T1 Wrought Alloy (UNS M11311)
Magnesium AZ31B, Extruded Hollow Shapes

MMAZ33 / 12315

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.