MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ravago Manufacturing Americas Aquatuf® HMP-337 (Roto) HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: HMP-337 is a high-density polyethylene compound designed for applications like kayaks or boats that require a balance high stiffness and extreme toughness.

Key Features: 35-mesh powder; Good moldability; Excellent long term outdoor weatherability (UV15); Superior balance of toughness and rigidity; Very high stiffness; Excellent low temperature impact; Compounded for uniform additive dispersion; Natural as well as standard, custom or special effect colors available; Stock colors may be available. See Stock color bulletin; Also available in pellet form as HM-337

Availability: North America

Features: Good Moldability; Good Toughness; Good Weather Resistance; High Rigidity; High Stiffness; Low Temperature Impact Resistance

Appearance: Colors Available; Opaque

Form: Powder

Processing Method: Rotational Molding

Information provided by Ravago Manufacturing Americas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.340 g/cc35-mesh powder; ASTM D1895
Density 0.951 g/ccASTM D792
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Flexural Modulus 150000 psiTangent, Rotational Molded; ASTM D790
Impact Test 60.0 ft-lb
@Temperature -40.0 °C
Rotational Molded, F50
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 140 °FUnannealed, Rotational Molded; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 104 °FUnannealed, Rotational Molded; ASTM D648
Flammability, UL94 HB
@Thickness 1.52 mm
 HB
@Thickness 3.05 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRAVAGO4851 / 311544

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.