MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECASINT 8591 grey Polytetrafluorethylene
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes:
  • very good slide and wear properties
  • low static friction
  • high dimensional stability
  • low outgassing
  • very good thermal stability
  • good chemical resistance
Target Industries:
  • aircraft and aerospace technology
  • cryogenic engineering
  • vacuum technology
  • propulsion technology

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.56 g/cc
Water Absorption 0.0030 %
@Time 86400 sec
DIN EN ISO 62
 0.016 %
@Time 346000 sec
DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 67DIN EN ISO 868
Tensile Strength 13.0 MPa50 mm/min; DIN EN ISO 527-1
Elongation at Break 20 %50 mm/min; DIN EN ISO 527-1
Modulus of Elasticity 2.30 GPa1 mm/min; DIN EN ISO 527-1
Coefficient of Friction 0.14 - 0.22
K (wear) Factor 100 - 1000 x 10-8 mm³/N-M
 
Thermal PropertiesOriginal ValueComments
CTE, linear 52.0 µm/m-°C
@Temperature 100 - 150 °C
XY; DIN EN ISO 11359-1;2
 53.0 µm/m-°C
@Temperature 23.0 - 100 °C
XY; DIN EN ISO 11359-1;2
 55.0 µm/m-°C
@Temperature 50.0 - 200 °C
XY; DIN EN ISO 11359-1;2
Maximum Service Temperature, Air 260 °Clong-term
Flammability, UL94 V-0DIN IEC 60695-11-10
 
Descriptive Properties
Colorgrey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIN8212 / 319140

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.