MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials Carbo-Rite™ M-530 High Impact Polystyrene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with Carbon Black Filler

Material Notes: Product Description: M-530 is a conductive carbon filled HIPS available as extruded sheet. Thermoformed trays are lightweight and easily thermoformed into deep pockets that maintain uniform static protection. It is high in stiffness and ensures uniform pocket formation when dimensional tolerance is critical. Product Format: M530 is available in customer extruded gauges from 0.012 to 0.08 inch and widths of 10 to 48 inches. Product is typically provided as rollstock with a smooth surface finished. Cut-sheets are also available.
Availability: Asia Pacific, Europe, Latin America, North America
Filler/Reinforcement: Carbon Black
Features: Consistent Performance; Durable; Electromagnetic Shielding (EMI); Cost-effective ESD protection; Recyclable Material
Uses: Electrical/Electronic Applications; Sheet; Tape
Appearance: Black
Forms: Sheet
Processing Method: Thermoforming

Information provided by Lubrizol Advanced Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.09 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 3480 psiASTM D638
Elongation at Break 10 %ASTM D638
Tensile Modulus 136000 psiASTM D638
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 900000 ohm-cmESD S11.12
Surface Resistance <= 7000 ohmESD S11.11
Static Decay 0.10 sec1000 V to 10 V, Charged Plate Monitor, 12% RH

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLUBR6009 / 268311

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.