MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Copper Alloy, UNS C14520, H02 Temper, Rod
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: ½ Hard

Fabrication Properties: Excellent Suitability - Soldering; Good Suitability – Brazing, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Fair Suitability - Oxyacetylene Welding, Gas Shielded Arc Welding, Butt Weld

Common Fabrication Processes: Cold - Drawing, machining, moderate cold heading; Hot - Extrusion, forging (closed die only)

Typical Uses: Fire Protection; Electrical Connectors; Motor Parts; Soldering Copper; Switch Parts; Transistor Bases; Forgings; Furnace Brazed Articles; Screw Machine Products; Wielding Torch Tips; Plumbing Fittings; Sprinkler Heads

Applicable Specifications: Bar – ASTM B301/B301M; Rod– ASTM B301/B301M; Shapes – ASTM B301/B301M; Wire – ASTM B301/B301M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.323 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 42
@Thickness 50.8 mm
 42
@Thickness 25.4 mm
 43
@Thickness 12.7 mm
 43
@Thickness 6.35 mm
Hardness, Rockwell 30T 50
Tensile Strength 42.0 ksi
@Thickness 50.8 mm
 42.0 ksi
@Thickness 25.4 mm
 43.0 ksi
@Thickness 12.7 mm
 43.0 ksi
@Thickness 6.35 mm
Tensile Strength, Yield 39.0 ksi
@Thickness 50.8 mm
0.2% Offset
 40.0 ksi
@Thickness 12.7 mm
0.2% Offset
 40.0 ksi
@Thickness 6.35 mm
0.2% Offset
 40.0 ksi
@Thickness 25.4 mm
0.2% Offset
Elongation at Break 18 %
@Thickness 6.35 mm
 20 %
@Thickness 12.7 mm
 25 %
@Thickness 25.4 mm
 35 %
@Thickness 50.8 mm
Tensile Modulus 17000 ksi
Modulus of Rigidity 6400 ksi
Poissons Ratio 0.33Calculated
Machinability 85 %
Forgeability 65 %
Shear Strength 25.0 ksi
@Thickness 50.8 mm
 25.0 ksi
@Thickness 25.4 mm
 26.0 ksi
@Thickness 12.7 mm
 26.0 ksi
@Thickness 6.35 mm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 ohm-cm85% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.50 µin/in-°F
@Temperature 20.0 - 100 °C
 9.70 µin/in-°F
@Temperature 20.0 - 200 °C
 9.90 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0920 BTU/lb-°F
Melting Point 1924 - 1967 °F
Solidus 1924 °F
Liquidus 1967 °F
Annealing Point 800 - 1200 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1400 - 1600 °FStress Relief
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu >= 99.9 %
Phosphorus, P 0.0040 - 0.020 %
Tellurium, Te 0.40 - 0.70 %
 
Descriptive Properties
Cold Work (%)152
 200.25
 200.5
 201
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC14520x1 / 291546

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.