MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Master Bond UV15-7TK1ANV One component, paste consistency UV curable system
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Stays in place when applied
  • Superb adhesive, sealant
  • Superior physical strength properties
  • Enhanced toughness and durability
Master Bond UV15-7TK1ANV is a one component UV curable polymer system with a paste consistency for high performance bonding, sealing and special encapsulation. This system is 100% reactive and does not contain any solvents or diluents. Its most salient features include superior physical strength properties, low shrinkage upon curing and enhanced non-yellowing stability. UV15-7TK1ANV offers very good chemical resistance to water, fuels, and oils, among others. It exhibits an exceptional combination of properties including outstanding durability, and good electrical insulation properties, along with fine thermal cycling capabilities. UV15-7TK1ANV bonds well to a wide variety of substrates including glass, metals and plastics, including polycarbonates, acrylics and polyester films. UV15-7TK1ANV is translucent and has a service temperature range of -80°F to +300°F. Master Bond UV15-7TK1ANV system is not oxygen inhibited and cures readily in 10-20 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output of 20 milliwatts/cm². No solvents or vapors are released during the curing process. The rate of cure depends upon the compound’s distance from the light source, the thickness of the section and, of course, the intensity of the light source. It should be noted that the system can cure in sections up to 1/8 inch. However, when bonding, sections of a few thousandths of an inch are more than adequate. This system can be used in optical, fiberoptic, electronic, laser, microelectronic and semiconductor applications, when a robust UV curable paste consistency system is desirable.

Product Advantages:

  • One component system; no mixing needed
  • Fast curing mechanism upon exposure to UV light
  • No air inhibition while curing; no special inert atmosphere required
  • Good dimensional stability and electrical insulation properties
  • High bond strength to many substrates
  • Paste-like consistency

Information provided by Masterbond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70 - 80
Tensile Strength 5000 - 6000 psi
Tensile Modulus 300000 - 350000 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cm
Dielectric Constant 3.4
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 55.0 - 60.0 µm/m-°C
Maximum Service Temperature, Air 300 °F
Minimum Service Temperature, Air -80.0 °F
Glass Transition Temp, Tg 65.0 - 70.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 MonthIn original unopened containers
 
Descriptive Properties
Colortranslucentcured
Viscositythixotropic paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMASTM734 / 233791

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.