Teijin® Tetoron® G2 is a polyester film which has high clarity and good slip characteristics. Teijin® Tetoron® G2 is available in the following variations: G2: Non-pretreated G2N: Adhesion Pretreated (one side) G2C: Corona Treated (one side) G2Z: Release Pretreated (one side) Typical Applications: Teijin® Tetoron® G2 is suitable for applications where low haze and good handling are desired product qualities. Intended applications include: - Labels
- Release Films
- Holograms
- Dry Film Resist (DFR)
Information provided by DuPont. |