MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil Mobil Polyrex EP 2
Categories: Fluid; Lubricant; Urea Gellant

Material Notes: Mobil Polyrex EP 2 is a shear-stable polyurea grease with excellent extreme-pressure (EP) and load-carrying characteristics. The proprietary polyurea thickener system exhibits excellent resistance to oxidation and oil separation at operating temperatures as high as 350°F. With its outstanding high-temperature oxidation stability, load-carrying capability, shear stability, water resistance and wide operating temperature range, Mobil Polyrex EP 2 is an excellent multi-purpose grease for a wide array of industrial and construction applications.

Mobil Polyrex EP 2 is an excellent multi-purpose grease for a wide array of industrial and construction applications.

Key Words: NLGI Grade 2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 85Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 235 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 18.4 cStASTM D445
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 500 kgASTM D2596
Four Ball Wear 0.400 mm40 kg, 1200 rpm, 75°C, 1 hr
Penetration 280Worked, 60x; ASTM D217
 310Worked, 100000, mm/10; ASTM D217
Oil Separation <= 0.30 %ASTM D1742
Timken Test 45.0 lb
 
Thermal PropertiesOriginal ValueComments
Dropping Point 280 °CASTM D2265
 
Descriptive Properties
Colorgreen
Corrosion Prevention, ASTM D1743pass
Grease Life, DIN 51821 (FE-9), hours490@ 177°C
Low Temperature Torque, ASTM D1478, g-cm12.2@ -40°C
Soap/Thickener Typepolyurea
Water Spray Resistance, ASTM D4049, % Spray-off15
Water Washout, ASTM D1264, wt%2.7@ 79°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Mobil Polyrex EM
AISI E 52100 Steel (100Cr6, SUJ2, UNS G52986)
AISI 1018 Steel, cold drawn
ExxonMobil Unirex N 3
ExxonMobil Mobil Polyrex EM 103

WEXXON406 / 75831

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.