MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
ITW Devcon® HV Tile Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: High-strength towelable adhesive compound designed for bonding ceramic tile to vertical, curved and overhead surfaces and repairing ceramic tile surfaces. Uses: Bonding ceramic tile to vertical, curved and overhead surfaces. Features: Non-sagging adhesive that will support 4 lbs. per square foot while curing, Fills gaps and joints in crushers prior to pouring backing compounds, Excellent adhesion to metal, ceramic and concrete, Easy to use 1:1 formula.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccCured
Solids Content 100 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 81
Modulus of Elasticity 5.52 GPa
Flexural Strength 5400 psiASTM D790
Compressive Strength 11800 psiASTM D695
Adhesive Bond Strength 1825 psiAdhesive Tensile Shear; ASTM D1002
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 45ASTM D150
Dielectric Strength 12.6 kV/mmASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.0 µin/in-°FASTM D696
Thermal Conductivity 1.25 W/m-K
Maximum Service Temperature, Air 200 °F
Shrinkage 0.10 %Linear During cure; ASTM D2566
 
Processing PropertiesOriginal ValueComments
Cure Time 8.00 hour
@Temperature 24.0 °C
Functional cure
 168 hour
@Temperature 24.0 °C
As Tested
Pot Life 35.0 min
@Temperature 23.9 °C
 
Descriptive Properties
ColorGrayCured
Coverage76 sq.in/lbCured @ 1/4" thick
Mix Ratio by volume1:1
Mix Ratio by weight1.1:1
Recoat Time11 to 16 hrs
Specific Volume (in.³/lb)19Cured
ViscosityNon-sag putty. Mixed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWD9179 / 239689

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.