MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lord Adhesives 6100HV Silver Conductor
Categories: Polymer; Thermoset; Epoxy; Epoxy, Electrically Conductive

Material Notes: LORD® 6100HV silver conductor is a one-component, thermosetting conductive epoxy designed primarily for surface mount attachment of electronic component devices. It is recommended for die attach and discrete component surface mount applications.

Features: may be applied by screen printing or syringe. cured film provides superior electrical and mechanical properties with excellent bonding to many types of materials, including epoxy laminate and alumina. solvent-free paste with excellent handling properties.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 330000 - 360000 cP
@Temperature 25.0 °C
Brookfield RVT, Spindle 7, 10 rpm
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 8000 - 10000 psiDie Shear, Bear Si die on alumina
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature -20.0 °C
from date of shipment in original, unopened container away from heat or flames
 
Descriptive Properties
AppearanceSilver Paste
Resistivity50 maxmohms/sq/mil, dried at room temp for 15 min
 50 maxcured at 150C for 30 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trelleborg Emerson & Cuming Eccobond® 57C Two-Component Silver Filled Electrically Conductive Epoxy Adhesive
Toho Tenax Besfight® G40-800 6K IMA-5C EP03 Continuous Filament Carbon Fiber
Toho Tenax Besfight® G30-500 6K HTA-7C EP01 Continuous Filament Carbon Fiber
Solvay Thornel® T-300 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
SGL Carbon Group PANOX® SA T320 EEA High performance oxidized textile fiber, Continuous Tow with 320k filaments

PLORD9332 / 232688

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.