MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Dow ELITE™ 5230F PE
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description: ELITE™ 5230F Enhanced Polyethylene Resin is produced via INSITE™ Technology from Dow. This resin offers high impact strength and good puncture resistance at moderate stretch levels for irregularly shapes loads. In addition, this resin provides excellent extensibility for higher yields on regular loads.
  • Excellent extensibility
  • High impact and puncture resistance

Availability: Latin America; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA FCN 424

Form: Pellets

Processing Method: Cast Film

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccASTM D792
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Puncture Resistance 11.0 lb (f)
@Thickness 0.0203 mm
Film Tensile Strength at Yield, MD 1320 psi
@Thickness 0.0203 mm
ASTM D882
Film Tensile Strength at Yield, TD 1220 psi
@Thickness 0.0203 mm
ASTM D882
Film Elongation at Break, MD 540 %
@Thickness 0.0203 mm
ASTM D882
Film Elongation at Break, TD 720 %
@Thickness 0.0203 mm
ASTM D882
Elongation, Ultimate 330 %
@Thickness 0.0203 mm
On-pallet testing
Elmendorf Tear Strength MD 310 g
@Thickness 0.0203 mm
ASTM D1922
Elmendorf Tear Strength TD 510 g
@Thickness 0.0203 mm
ASTM D1922
Dart Drop Test 320 g
@Thickness 0.0203 mm
ASTM D1709B
Film Tensile Strength at Break, MD 6670 psi
@Thickness 0.0203 mm
ASTM D882
Film Tensile Strength at Break, TD 5520 psi
@Thickness 0.0203 mm
ASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 252 °F
 
Optical PropertiesOriginal ValueComments
Haze 0.50 %
@Thickness 0.0203 mm
ASTM D1003
Gloss 95 %45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 520 °FExtrusion
 
Descriptive Properties
Film Puncture Resistance326 ft-lb/in30.8 mil

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF499 / 311192

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.