MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Mallard Creek Polymers Ecronova® 6608 Acrylic Emulsion
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Ecronova® 6608 is an ambient cure, pure acrylic emulsion that incorporates excellent block and alkaline resistance and extraordinary wet adhesion with minimal water absorption. The product displays early water resistance and very good weathering, as well as a non-yellowing elastic film. This emulsion shows excellent adhesion to difficult substrates such as metals and plastics. This emulsion is APEO free.

Markets: Paints and Coatings

Applications: Wood Coating, Metal Coating

Related Products: Ecronova 6630, Ecronova 6620

Information provided by Mallard Creek Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 42.5 - 43.5 %42.5 - 43.5 %
pH 7.7 - 8.27.7 - 8.2
Viscosity <= 300 cP<= 300 cP
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 23.0 °C73.4 °F
 
Descriptive Properties
Minimum Film Formation Temperature (°C)10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMCP9901 / 250405

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.