System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
SABIC LNP™ LUBRICOMP™ Compound QL002 Polyamide 610 (Nylon 610)
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 610 (PA610)
Material Notes:
LNP LUBRICOMP QL002 compound is based on Nylon 6/10 resin containing 10% PTFE. Added features of this grade include: Wear Resistant.
Features: Wear resistant
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.15
g/cc
1.15
g/cc
ASTM D792
Density
1.14
g/cc
0.0412
lb/in³
ASTM D792
Moisture Absorption
0.120 - 0.200 %
0.120 - 0.200 %
Injection Molding
0.260 %
0.260 %
23°C/50% RH/24 hrs; ASTM D570
0.380 %
0.380 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow
0.0090
-
0.030
cm/cm
0.0090
-
0.030
in/in
24hrs; ASTM D955
Linear Mold Shrinkage, Transverse
0.010
-
0.040
cm/cm
0.010
-
0.040
in/in
24hrs; ASTM D955
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
52.0
MPa
7540
psi
5 mm/min; ASTM D638
61.0
MPa
8850
psi
5 mm/min; ISO 527
Elongation at Break
2.3 %
2.3 %
5 mm/min; ASTM D638
4.5 %
4.5 %
5 mm/min; ISO 527
Tensile Modulus
2.48
GPa
360
ksi
1 mm/min; ISO 527
2.68
GPa
389
ksi
50 mm/min; ASTM D638
Flexural Strength
73.0
MPa
10600
psi
ISO 178
Flexural Modulus
2.04
GPa
296
ksi
2 mm/min; ISO 178
2.27
GPa
329
ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched
39.0
J
28.8
ft-lb
ASTM D256
Izod Impact, Unnotched
3.99
J/cm
7.47
ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO)
4.00
kJ/m²
1.90
ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
42.0
kJ/m²
20.0
ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy
3.00
J
2.21
ft-lb
ASTM D3763
Coefficient of Friction, Dynamic
0.38
0.38
ASTM D3702 Modified: Manual
Coefficient of Friction, Static
0.25
0.25
ASTM D3702 Modified: Manual
K (wear) Factor
70.5
x 10
-8
mm³/N-M
35.0
x 10
-10
in³-min/ft-lb-hr
Washer; ASTM D3702 Modified: Manual
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
110
µm/m-°C
@Temperature -30.0 - 30.0 °C
61.1
µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow
120
µm/m-°C
@Temperature -30.0 - 30.0 °C
66.7
µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi)
143
°C
289
°F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
164
°C
@Thickness 3.20 mm
327
°F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
54.0
°C
129
°F
Flatw 80*10*4 sp=64mm; ISO 75/Af
63.0
°C
@Thickness 3.20 mm
145
°F
@Thickness 0.126 in
unannealed; ASTM D648
Processing Properties
Metric
English
Comments
Zone 2
260
-
270
°C
500
-
518
°F
Zone 3
270
-
280
°C
518
-
536
°F
Melt Temperature
270
-
275
°C
518
-
527
°F
Injection Molding
Mold Temperature
80.0
-
95.0
°C
176
-
203
°F
Drying Temperature
80.0
°C
176
°F
Injection Molding
Dry Time
4.00
hour
4.00
hour
Injection Molding
Back Pressure
0.200
-
0.300
MPa
29.0
-
43.5
psi
Screw Speed
30
-
60
rpm
30
-
60
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PSABH80952 / 288899
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.