MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Phillips 66 Diamond Class® C/S 32 Heat Transfer Fluid
Categories: Fluid; Lubricant

Material Notes: Diamond Class Heat Transfer Fluids are premium quality fluids specifically developed for use in liquid-phase heat transfer systems. They are available in two different formulations, designated “O/S” for use in open systems and “C/S” for use in closed systems. Diamond Class Heat Transfer Fluids O/S and C/S are formulated with premium hydrocracked paraffinic base oils and advanced additive chemistry to provide outstanding thermal stability and low sludge-forming tendency for long service life and outstanding overall performance.

Applications: Diamond Class Heat Transfer Fluid O/S is optimized for use in pressure-relieved, liquid-phase heat transfer systems with expansion tanks, where there is the possibility of contact between the heat transfer fluid and air in the expansion tank. It is fortified with oxidation and corrosion inhibitors to prevent fluid degradation and deposit buildup in the system. The O/S fluid is recommended for use in systems operating with continuous maximum bulk oil temperatures up to 550°F (290°C), intermittent maximum temperatures as high as 650°F (343°C), and a maximum skin film temperature of 600°F (316°C). Diamond Class Heat Transfer Fluid C/S is optimized for use in pressure-relieved, expansion tank-equipped liquid-phase heat transfer systems that are closed to the atmosphere and potential air contamination. The system must be equipped with a cold-oil seal pot on the expansion tank vent, or operated with low-pressure nitrogen blanketing of the oil so there is no possibility of air contacting the oil during operation. The C/S fluid is fortified with special additives to prevent thermal degradation. It is recommended for use in systems operating with continuous maximum bulk oil temperatures up to 620°F (327°C) and maximum skin film temperatures up to 650°F (343°C). Some common applications include:

  • Liquid-phase heat transfer systems
  • Heat transfer medium for industrial manufacturing processes
  • Heat transfer equipment used in the manufacture of resins and coatings
  • Asphalt heating
  • Die casting
  • Plastic injection molding and extrusion
  • Wax coating equipment
Features/Benefit:
  • Outstanding performance in closed or open systems
  • Outstanding thermal stability to minimize deposits
  • Long service life
  • Less waste oil disposal
  • Reduced operating costs

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.862 g/cc
Density 7.18 lb/gal
Viscosity Measurement 102Index
Viscosity Measure 0.69 cSt
@Temperature 316 °C
Kinematic
 0.91 cSt
@Temperature 260 °C
Kinematic
 1.35 cSt
@Temperature 204 °C
Kinematic
Kinematic Viscosity at 40°C (104°F) 32 cSt
Kinematic Viscosity at 100°C (212°F) 5.4 cSt
Oxidative Stability 7.47 hourRPVOT; ASTM D2272
ASTM Color 0.50ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.010[mg KOH/g]; ASTM D974
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 290 °C
 343 °C
Pour Point -42.0 °C
Flash Point 225 °CCOC
Ignition Temperature 364 °CAutoignition; ASTM E659
 
Descriptive Properties
Carbon Residue<0.1%ASTM D524
Copper Corrosion1aASTM D130

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5167 / 198420

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.