Physical Properties | Metric | English | Comments |
---|
Density | 0.970 g/cc | 0.0350 lb/in³ |
| 1.16 g/cc | 0.0419 lb/in³ |
| 1.16 g/cc | 0.0419 lb/in³ |
Viscosity | 42 cP @Temperature 22.0 °C | 42 cP @Temperature 71.6 °F |
| 250 cP @Temperature 48.9 °C | 250 cP @Temperature 120 °F |
| 750 cP @Temperature 29.4 °C | 750 cP @Temperature 84.9 °F |
| 765 cP @Temperature 29.0 °C | 765 cP @Temperature 84.2 °F |
| 1124 cP @Temperature 25.0 °C | 1124 cP @Temperature 77.0 °F |
| 1367 cP @Temperature 22.0 °C | 1367 cP @Temperature 71.6 °F |
| 3000 cP @Temperature 15.6 °C | 3000 cP @Temperature 60.1 °F |
| 6890 cP @Temperature 22.0 °C | 6890 cP @Temperature 71.6 °F |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore D | 90 @Treatment Temp. 49.0 °C, Time 28800 sec | 90 @Treatment Temp. 120 °F, Time 8.00 hour |
| 91 @Treatment Temp. 22.0 °C, Time 2.42e+6 sec | 91 @Treatment Temp. 71.6 °F, Time 672 hour |
| 92 @Treatment Temp. 25.0 °C, Time 1.21e+6 sec | 92 @Treatment Temp. 77.0 °F, Time 336 hour |
| 92 @Treatment Temp. 60.0 °C, Time 28800 sec | 92 @Treatment Temp. 140 °F, Time 8.00 hour |
| 94 @Treatment Temp. 82.0 °C, Time 28800 sec | 94 @Treatment Temp. 180 °F, Time 8.00 hour |
Tensile Strength | 59.3 MPa @Treatment Temp. 22.0 °C, Time 2.42e+6 sec | 8600 psi @Treatment Temp. 71.6 °F, Time 672 hour |
| 65.9 MPa @Treatment Temp. 25.0 °C, Time 1.21e+6 sec | 9560 psi @Treatment Temp. 77.0 °F, Time 336 hour |
| 75.8 MPa @Treatment Temp. 49.0 °C, Time 28800 sec | 11000 psi @Treatment Temp. 120 °F, Time 8.00 hour |
| 75.8 MPa @Treatment Temp. 60.0 °C, Time 28800 sec | 11000 psi @Treatment Temp. 140 °F, Time 8.00 hour |
| 75.8 MPa @Treatment Temp. 82.0 °C, Time 28800 sec | 11000 psi @Treatment Temp. 180 °F, Time 8.00 hour |
Elongation at Break | 1.7 % @Treatment Temp. 22.0 °C, Time 2.42e+6 sec | 1.7 % @Treatment Temp. 71.6 °F, Time 672 hour |
| 2.1 % @Treatment Temp. 25.0 °C, Time 1.21e+6 sec | 2.1 % @Treatment Temp. 77.0 °F, Time 336 hour |
| 3.6 % @Treatment Temp. 49.0 °C, Time 28800 sec | 3.6 % @Treatment Temp. 120 °F, Time 8.00 hour |
| 4.4 % @Treatment Temp. 60.0 °C, Time 28800 sec | 4.4 % @Treatment Temp. 140 °F, Time 8.00 hour |
| 5.9 % @Treatment Temp. 82.0 °C, Time 28800 sec | 5.9 % @Treatment Temp. 180 °F, Time 8.00 hour |
Tensile Modulus | 3.07 GPa | 445 ksi |
| 3.39 GPa | 491 ksi |
| 3.50 GPa | 507 ksi |
| 3.69 GPa | 535 ksi |
| 4.01 GPa | 582 ksi |
Flexural Strength | 101 MPa @Treatment Temp. 22.0 °C, Time 2.42e+6 sec | 14600 psi @Treatment Temp. 71.6 °F, Time 672 hour |
| 104 MPa @Treatment Temp. 25.0 °C, Time 1.21e+6 sec | 15100 psi @Treatment Temp. 77.0 °F, Time 336 hour |
| 136 MPa @Treatment Temp. 49.0 °C, Time 28800 sec | 19700 psi @Treatment Temp. 120 °F, Time 8.00 hour |
| 138 MPa @Treatment Temp. 60.0 °C, Time 28800 sec | 20000 psi @Treatment Temp. 140 °F, Time 8.00 hour |
| 140 MPa @Treatment Temp. 82.0 °C, Time 28800 sec | 20300 psi @Treatment Temp. 180 °F, Time 8.00 hour |
Flexural Modulus | 3.23 GPa @Treatment Temp. 82.0 °C, Time 28800 sec | 469 ksi @Treatment Temp. 180 °F, Time 8.00 hour |
| 3.57 GPa @Treatment Temp. 60.0 °C, Time 28800 sec | 518 ksi @Treatment Temp. 140 °F, Time 8.00 hour |
| 3.78 GPa @Treatment Temp. 49.0 °C, Time 28800 sec | 548 ksi @Treatment Temp. 120 °F, Time 8.00 hour |
| 3.93 GPa @Treatment Temp. 25.0 °C, Time 1.21e+6 sec | 570 ksi @Treatment Temp. 77.0 °F, Time 336 hour |
| 3.96 GPa @Treatment Temp. 22.0 °C, Time 2.42e+6 sec | 575 ksi @Treatment Temp. 71.6 °F, Time 672 hour |
Compressive Yield Strength | 103 MPa @Treatment Temp. 49.0 °C, Time 28800 sec | 14900 psi @Treatment Temp. 120 °F, Time 8.00 hour |
| 103 MPa @Treatment Temp. 60.0 °C, Time 28800 sec | 14900 psi @Treatment Temp. 140 °F, Time 8.00 hour |
| 103 MPa @Treatment Temp. 82.0 °C, Time 28800 sec | 14900 psi @Treatment Temp. 180 °F, Time 8.00 hour |
| 108 MPa @Treatment Temp. 22.0 °C, Time 2.42e+6 sec | 15700 psi @Treatment Temp. 71.6 °F, Time 672 hour |
| 111 MPa @Treatment Temp. 25.0 °C, Time 1.21e+6 sec | 16100 psi @Treatment Temp. 77.0 °F, Time 336 hour |
|
Thermal Properties | Metric | English | Comments |
---|
Deflection Temperature at 0.46 MPa (66 psi) | 53.9 °C @Treatment Temp. 22.0 °C, Time 2.42e+6 sec | 129 °F @Treatment Temp. 71.6 °F, Time 672 hour |
| 53.9 °C @Treatment Temp. 25.0 °C, Time 1.21e+6 sec | 129 °F @Treatment Temp. 77.0 °F, Time 336 hour |
| 67.8 °C @Treatment Temp. 49.0 °C, Time 28800 sec | 154 °F @Treatment Temp. 120 °F, Time 8.00 hour |
| 74.4 °C @Treatment Temp. 60.0 °C, Time 28800 sec | 166 °F @Treatment Temp. 140 °F, Time 8.00 hour |
| 92.2 °C @Treatment Temp. 82.0 °C, Time 28800 sec | 198 °F @Treatment Temp. 180 °F, Time 8.00 hour |
Glass Transition Temp, Tg | 97.8 °C | 208 °F |
| 56.7 °C @Treatment Temp. 22.0 °C, Time 2.42e+6 sec | 134 °F @Treatment Temp. 71.6 °F, Time 672 hour |
| 56.7 °C @Treatment Temp. 25.0 °C, Time 1.21e+6 sec | 134 °F @Treatment Temp. 77.0 °F, Time 336 hour |
| 62.2 °C @Treatment Temp. 22.0 °C, Time 2.42e+6 sec | 144 °F @Treatment Temp. 71.6 °F, Time 672 hour |
| 64.4 °C @Treatment Temp. 25.0 °C, Time 1.21e+6 sec | 148 °F @Treatment Temp. 77.0 °F, Time 336 hour |
| 68.9 °C @Treatment Temp. 49.0 °C, Time 28800 sec | 156 °F @Treatment Temp. 120 °F, Time 8.00 hour |
| 71.1 °C @Treatment Temp. 22.0 °C, Time 2.42e+6 sec | 160 °F @Treatment Temp. 71.6 °F, Time 672 hour |
| 72.8 °C @Treatment Temp. 25.0 °C, Time 1.21e+6 sec | 163 °F @Treatment Temp. 77.0 °F, Time 336 hour |
| 76.1 °C @Treatment Temp. 49.0 °C, Time 28800 sec | 169 °F @Treatment Temp. 120 °F, Time 8.00 hour |
| 77.2 °C @Treatment Temp. 60.0 °C, Time 28800 sec | 171 °F @Treatment Temp. 140 °F, Time 8.00 hour |
| 85.6 °C @Treatment Temp. 60.0 °C, Time 28800 sec | 186 °F @Treatment Temp. 140 °F, Time 8.00 hour |
| 86.7 °C @Treatment Temp. 49.0 °C, Time 28800 sec | 188 °F @Treatment Temp. 120 °F, Time 8.00 hour |
| 92.2 °C @Treatment Temp. 82.0 °C, Time 28800 sec | 198 °F @Treatment Temp. 180 °F, Time 8.00 hour |
| 96.7 °C @Treatment Temp. 60.0 °C, Time 28800 sec | 206 °F @Treatment Temp. 140 °F, Time 8.00 hour |
| 104 °C @Treatment Temp. 82.0 °C, Time 28800 sec | 219 °F @Treatment Temp. 180 °F, Time 8.00 hour |
| 113 °C @Treatment Temp. 82.0 °C, Time 28800 sec | 236 °F @Treatment Temp. 180 °F, Time 8.00 hour |
|
Processing Properties | Metric | English | Comments |
---|
Cure Time | 240 - 300 min | 4.00 - 5.00 hour |
Pot Life | 33.0 - 41.0 min @Load 0.500 kg, Temperature 29.0 °C | 33.0 - 41.0 min @Load 1.10 lb, Temperature 84.2 °F |
| 35.0 - 43.0 min @Load 0.500 kg, Temperature 22.0 °C | 35.0 - 43.0 min @Load 1.10 lb, Temperature 71.6 °F |
| 36.0 - 45.0 min @Load 0.150 kg, Temperature 29.0 °C | 36.0 - 45.0 min @Load 0.331 lb, Temperature 84.2 °F |
| 38.0 - 48.0 min @Load 0.500 kg, Temperature 25.0 °C | 38.0 - 48.0 min @Load 1.10 lb, Temperature 77.0 °F |
| 44.0 - 54.0 min @Load 0.150 kg, Temperature 25.0 °C | 44.0 - 54.0 min @Load 0.331 lb, Temperature 77.0 °F |
| 52.0 - 64.0 min @Load 0.150 kg, Temperature 22.0 °C | 52.0 - 64.0 min @Load 0.331 lb, Temperature 71.6 °F |
Working Life | 120 - 180 min | 120 - 180 min |
Shelf Life | 24.0 Month | 24.0 Month |
| 36.0 Month | 36.0 Month |
|
Descriptive Properties |
---|
Mix ratio | 100:25.8–100:30.1 |
| 100:27.7 |
| 100:31.1–100:36.3 |
| 100:33.3 |
| 3.00:1 |
| 3.21:1–2.75:1 |
| 3.5:1 |
| 3.87:1–3.32:1 |