Highly impact modified, heat stabilized Amodel® ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel® PPA resins, ET-1000 HS offers high fatigue strength, good chemical resistance and high mechanical property retention over a broad temperature and humidity range. - Natural: ET-1000 HS NT Markets/Uses: Automotive / Automotive E/E / Engine Sensors; Automotive / Automotive E/E / Sensors; Automotive / Automotive E/E / Wire Harness Connectors Applications: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Connectors; General Purpose; Housings; Industrial Applications; Industrial Parts; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal Replacement Features: Chemical Resistant; Ductile; Heat Stabilized; Hot Water Moldability; Impact Modified; Low Warpage Injection notes: MOLD TEMPERATURE - If the wall is thick, lower temperatures may be used to prevent ejector pin problems. STORAGE: - Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® processing guide. Information provided by Solvay Specialty Polymers. |