MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lord Adhesives Accelerator 6 and 6B Accelerator
Categories: Other Engineering Material; Catalyst/Initiator

Material Notes: LORD® Accelerator 6 and 6GB are mix-in curatives designed for use with LORD acrylic adhesives. LORD Accelerator 6 and 6GB, when mixed with LORD 600 series acrylic adhesives, create adhesive systems that will bond a variety of prepared or unprepared metals and plastics. LORD Accelerator 6GB allows precise control of adhesive bondline thickness due to its content of glass beads, 0.01” (0.025 cm) diameter.

Features: provides room temperature cure with all LORD 600 series acrylic adhesives. contains no solvent, non-flammable and virtually odorless. resists common environmental conditions when used with LORD acrylic adhesives.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 12.0 - 12.9 lb/galAccelerator 6
 12.0 - 13.0 lb/galAccelerator 6GB
Solids Content 95.52 %Accelerator 6GB, by weight
 96.34 %Accelerator 6, by weight
Viscosity Measure 50000 - 350000 cStAccelerator 6GB, HAT T-C, 5 rpm
 50000 - 350000 cSt
@Temperature 25.0 °C
Accelerator 6, HAT T-C, 5 rpm
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 93.0 °CSeta, both materials
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature 4.00 - 10.0 °C
both materials, in original, unopened container
 
Descriptive Properties
AppearanceGrey PasteAccelerator 6
 Grey to Black PasteAccelerator 6GB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD9104 / 232493

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.