MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Akrochem CIMBAR™ 325
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CIMBAR barite products are made using only the highest quality white, natural barium sulfate ore. CIMBAR barites unique properties of fine grind, high specific gravity, low solubility and chemical inertness make them ideal for many applications.

Uses:
Coatings: Automotive Primers; Automotive Topcoats; High Gloss Enamel; Powder Coatings; Semi-Gloss Latexes; Gloss Latexes; Industrial Coatings; Architectural Coatings; Maintenance Coatings; Industrial Primers
Fillers: Plastics; Ceramics; Friction Materials; Rubber Goods; Plastisols; Adhesives; Latex products; Urethane Foams; Acoustical Compounds; Insulating Materials; Sound Attenuation Products

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 4.40 g/cc
Bulk Density 0.961 g/ccLoose
 2.40 g/ccCompacted
Particle Size 8.5 µmMedian
 40 µmTop size
Particle Mesh Size 325 Mesh0.2% retained
pH 8.5
 
Processing PropertiesOriginal ValueComments
Moisture Content 0.10 %
 
Component Elements PropertiesOriginal ValueComments
Al2O3 0.010 %
Fe2O3 0.020 %
Loss on Ignition(%) 0.75 %
 
Descriptive Properties
Absorption9
Color93L (CIE)
Content0.0005Total Heavy Metals
 0.0082Total Silicates
 0.98BaSO4
Hegman Fineness4.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH340 / 315258

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.