MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Essentium PCTG-Z Additive Manufacturing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyester, TP; Polycyclohexylenedimethylene Terephthalate (PCT); Glycol-Modified PCT (PCTG) Copolyester

Material Notes: All-purpose material for ESD safe jigs and fixtures; Non-marring; Low cost; Easy to print; Good all-around mechanical properties

Information provided by Essentium Materials, LLC.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 33.0 MPaYX Orientation; ISO 527-2
 33.3 MPaZX Orientation; ISO 527-2
 41.0 MPa45/45 Orientation; ISO 527-2
 45.0 MPaXY Orientation; ISO 527-2
Elongation at Break 2.2 %ZX Orientation; ISO 527-2
 2.8 %YX Orientation; ISO 527-2
 8.8 %45/45 Orientation; ISO 527-2
 150 %XY Orientation; ISO 527-2
Modulus of Elasticity 1.61 GPaYX Orientation; ISO 527-2
 1.67 GPaZX Orientation; ISO 527-2
 1.74 GPa45/45 Orientation; ISO 527-2
 1.81 GPaXY Orientation; ISO 527-2
Flexural Strength 37.2 MPaYX Orientation; ISO 527-2
 46.8 MPaZX Orientation; ISO 527-2
 64.6 MPa45/45 Orientation; ISO 527-2
 74.5 MPaXY Orientation; ISO 527-2
Flexural Modulus 1420 MPaYX Orientation; ISO 527-2
 1490 MPa45/45 Orientation; ISO 527-2
 1590 MPaZX Orientation; ISO 527-2
 1720 MPaXY Orientation; ISO 527-2
Izod Impact, Notched (ISO) 2.10 kJ/m²ZX Orientation; ISO 180/A
 2.70 kJ/m²45/45 Orientation; ISO 180/A
 3.30 kJ/m²YX Orientation; ISO 180/A
 7.00 kJ/m²XY Orientation; ISO 180/A
 
Thermal PropertiesOriginal ValueComments
Melting Point 202 °CASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °CISO 75
Glass Transition Temp, Tg 76.0 °CASTM D3418

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PESSEN910 / 291042

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.