MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Celanese Zytel® FN718 BK230A PA66-F
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Flexible Polyamide 66

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³DAM; ISO 1183
Moisture Absorption 1.40 %
@Thickness 2.00 mm
1.40 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Stress at Strain  21.0 MPa
@Strain 50 %
3050 psi
@Strain 50 %
50% RH; ISO 527-1/-2
 33.0 MPa
@Strain 50 %
4790 psi
@Strain 50 %
DAM; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %50% RH; ISO 527-1/-2
 >= 50 %>= 50 %DAM; ISO 527-1/-2
Tensile Modulus 0.440 GPa63.8 ksi50% RH; ISO 527-1/-2
 0.900 GPa131 ksiDAM; ISO 527-1/-2
Flexural Modulus 0.900 GPa131 ksiDAM; ISO 178
Poissons Ratio 0.450.45DAM
 0.470.4750% RH
Izod Impact, Notched (ISO)  25.0 kJ/m²
@Temperature -40.0 °C
11.9 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 95.0 kJ/m²
@Temperature 23.0 °C
45.2 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
Charpy Impact, Notched  3.00 J/cm²
@Temperature -40.0 °C
14.3 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eA
 10.5 J/cm²
@Temperature 23.0 °C
50.0 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 263 °C505 °F10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °C154 °FDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FDAM; ISO 75-1/-2
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
<= 3.15 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 275 - 290 °C527 - 554 °FRange, Extrusion
 275 - 295 °C527 - 563 °FRange, Injection
 285 °C545 °FOptimum, Injection
Mold Temperature 60.0 °C140 °FOptimum, Injection
 40.0 - 80.0 °C104 - 176 °FInjection
Drying Temperature 80.0 °C176 °FInjection
 80.0 °C176 °FExtrusion
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
 4.00 - 6.00 hour4.00 - 6.00 hourExtrusion, Dehumidified Dryer
Moisture Content <= 0.060 %<= 0.060 %Extrusion
 <= 0.20 %<= 0.20 %Injection
 
Descriptive Properties
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
ISO designationISO 16396-PA66-F,,M1CG1,S14-010
Part Marking Code>PA66-F<ISO 11469
PolymerPA66...
Resin IdentificationPA66-FISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSX5409b / 291011

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.