MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ATSP Innovations NOWE™ Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: KEY CHARACTERISTICS:
  • Outstanding wear properties
  • Low coefficient of friction
  • High working temperature
  • Excellent oxidative stability ? Very low moisture pickup
  • Non-flammable
  • Cryogenic-safe
  • Easy machinability—low dust
NOWE™ uses a proprietary blend of ATSP polymer with reinforcements and solid lubricants. ATSP (aromatic thermosetting copolyester) is a new class of high performance polymer that has the best of both thermoset and thermoplastic systems. It has high dimensional stability and performance like thermosets while being recyclable like thermoplastics.

This data was provided by ATSP Innovations

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.45 g/cc
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 340 MPaISO 604
Compressive Modulus 8.50 GPaASTM D695
Coefficient of Friction 0.10 - 0.30typical dry; Maximum sliding speed 2.4 m/s
Limiting Pressure Velocity 1.00 MPa-m/sec
@Temperature 300 °C
 24.0 MPa-m/sec
@Temperature 25.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 µm/m-°C
Maximum Service Temperature, Air 370 °C
Maximum Service Temperature, Inert 425 °C
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PESTHR03 / 243008

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.