General Information: 20760 is a water based product for use in bonding PVC flooring to a plywood base. It is high solids and can be sprayed, brushed or roll coated. Application amounts vary according to substrates and are generally around 8-10 wet mils. Substrates must be wet mated and allowed to dry to develop sufficient bond for subsequent handling. Strength development is rapid (1.5-3 hrs.) at 700F and above. Full strength develops within 24 hours. Bondline is water resistance and has good resistant to plasticizer migration.Information provided by H.B. Fuller Company |