MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC VALOX 865 PBT+PET (Asia Pacific)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polyethylene Terephthalate (PET)

Material Notes: 30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855.

Information provided by SABIC Innovative Plastics for Asia Pacific.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.66 g/ccASTM D 792
Water Absorption 0.030 %
@Time 86400 sec
ASTM D 570
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
@Thickness 1.50 - 3.20 mm
SABIC Method
 0.0050 - 0.0080 cm/cm
@Thickness 3.20 - 4.60 mm
SABIC Method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm
@Thickness 1.50 - 3.20 mm
SABIC Method
 0.0060 - 0.0090 cm/cm
@Thickness 3.20 - 4.60 mm
SABIC Method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 119ASTM D 785
Tensile Strength at Break 117 MPaType I, 5 mm/min; ASTM D 638
Flexural Strength 179 MPa1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 7580 MPa1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 80.0 J/m
@Temperature 23.0 °C
ASTM D 256
Izod Impact, Unnotched 640 J/m
@Temperature 23.0 °C
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.80e+16 ohm-cmASTM D 257
Dielectric Constant 3.7
@Frequency 1e+6 Hz
ASTM D 150
 3.8
@Frequency 100 Hz
ASTM D 150
Dielectric Strength 18.8 kV/mm
@Thickness 3.20 mm
in air; ASTM D 149
 23.2 kV/mm
@Thickness 1.60 mm
in oil; ASTM D 149
Dissipation Factor 0.0020
@Frequency 100 Hz
ASTM D 150
 0.010
@Frequency 1e+6 Hz
ASTM D 150
Arc Resistance 60 - 120 secPLC 6; ASTM D 495
Comparative Tracking Index 175 - 250 VPLC 3; UL 746A
Hot Wire Ignition, HWI 60 - 120 secPLC 1; UL 746A
High Amp Arc Ignition, HAI 15 - 30 arcsPLC 3; UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minPLC 4; UL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 21.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
 21.6 µm/m-°C
@Temperature 60.0 - 138 °C
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 212 °C
@Thickness 6.40 mm
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 193 °C
@Thickness 6.40 mm
unannealed; ASTM D 648
UL RTI, Electrical 110 °CUL 746B
UL RTI, Mechanical with Impact 110 °CUL 746B
UL RTI, Mechanical without Impact 110 °CUL 746B
Flammability, UL94 V-0
@Thickness 1.80 mm
UL 94
 5VA
@Thickness 2.99 mm
UL 94

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BLUESTAR 403HF-G30 PBT, 30% Glass Filled
BLUESTAR 403HF-G20 PBT, 20% Glass Filled
BLUESTAR 403G-MG30 PBT, 30% Glass Filled
BLUESTAR 403G-MG20 PBT, 20% Glass Filled
BLUESTAR 203G30 PBT, 30% Glass Filled

PSABI48662 / 189753

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.