Hubercarb® Q Series products are mined and manufactured in Quincy, IL, USA and include fine, medium-fine and granular particle size calcium carbonates. This grade has been surface-modified to enhance end-use performance. Uses include cat litter to concrete to paint to plastics. Select Hubercarb Q products are also produced to meet the requirements for animal feed applications, providing a cost-effective source of calcium from the high purity limestone ore.Information provided by Huber Engineered Materials. |