MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Selenis VENUZ BD 187 Copolyester for Cosmetics Packaging
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Selenis Venuz BD 187 has been specifically developed for the cosmetics market where outstanding clarity, great performance and easy processing is the target. Cosmetic parts molded from Selenis Venuz BD 187 provide good chemical resistance to most ingredients used in the industry as well as good barrier properties, helping brand owners grant product safety and preservation during storage. Packaging cost may be reduced as shelf life can be maintained even without the use of additional PP-inserts as usual in SAN and PMMA thick wall jars. The clarity of Selenis Venuz BD 187 allows packaging engineers to design parts from thin to thick walls without sacrificing transparency. The combination of density and thick walls increases the weight of the package, reinforcing the consumer perception of a high-end quality product. Selenis Venuz BD 187 provides good impact resistance, resembling the appearance of glass, allowing unique and personalized designs. Selenis Venuz BD 187 copolyester is the ideal choice for thin wall injection molding applications. Due to the high flow characteristics of this material short cycle times improve efficiency and lower cost per part. For packaging containers, a minimum wall thickness of 0,6 mm can be targeted using Selenis Venuz BD 187. Selenis Venuz BD 187 is a ready-to-use product supplied with a demolding agent to ease process.

Information provided by Selenis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.730 g/cc0.0264 lb/in³
Density 1.27 g/cc0.0459 lb/in³ASTM D792
Water Absorption <= 0.12 %<= 0.12 %ASTM D570
Viscosity Test 63 - 67 cm³/g0.63 - 0.67 dl/gIntrinsic; ISO 1628-5
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/inASTM D 955
ASTM Color <= 1.0<= 1.0b*; ASTM D6290
 >= 68>= 68L*; ASTM D6290
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 47.0 MPa6820 psi(σm); ISO 527 -1/- 2
Tensile Strength, Yield 47.0 MPa6820 psi(σy); ISO 527 -1/- 2
Elongation at Break 58 %58 %Nominal, (εtb); ISO 527 -1/- 2
Elongation at Yield 4.3 %4.3 %(εm); ISO 527 -1/- 2
 4.3 %4.3 %(εy); ISO 527 -1/- 2
Tensile Modulus 1.952 GPa283.1 ksiISO 527 -1/- 2
Flexural Strength 60.0 MPa8700 psiISO 178
Flexural Modulus 1.894 GPa274.7 ksiISO 178
Izod Impact, Notched (ISO)  4.80 kJ/m²
@Temperature -30.0 °C
2.28 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
 4.90 kJ/m²
@Temperature 0.000 °C
2.33 ft-lb/in²
@Temperature 32.0 °F
ISO 180/A
 5.70 kJ/m²
@Temperature 23.0 °C
2.71 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/A
Izod Impact, Unnotched (ISO)  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 180/U
 NB
@Temperature 0.000 °C
NB
@Temperature 32.0 °F
ISO 180/U
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
50% RH; ISO 180/U
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 85.0 °C185 °FASTM D3418
 
Optical PropertiesMetricEnglishComments
Gloss 164 %164 %60º; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 250 °C356 - 482 °F
Drying Temperature <= 70.0 °C<= 158 °Fto avoid chips sticking together in dryer hopper
 65.0 °C
@Time 21600 - 28800 sec
149 °F
@Time 6.00 - 8.00 hour
Moisture Content <= 0.0040 %<= 0.0040 %dried
Dew Point -40.0 °C-40.0 °F
 
Descriptive Properties
Particle size320 ± 50 mg/20 chips
Pellet ShapeCylindrical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSELE927 / 243425

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.