MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ITW Devcon® Floor Patch™
Categories: Polymer; Thermoset

Material Notes: All-purpose concrete patching compound that bonds to concrete, brick, masonry, metal, or wood surfaces. Uses: Ideal for patching concrete, brick, masonry, floors, or retaining walls where the concrete has spalled. The material will also bond to wood and metal. Can be used to anchor bolts in concrete. Features: Easy to mix and apply, Trowelable to 1/4" or more, High compressive strength, Resistant to water, oils, solvents, and alkalis.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 100 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85
Compressive Strength 8000 psi
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 °FTemperature Resistance - Dry
 250 °FTemperature Resistance - Wet
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 90.0 °FApplication Temperature
Cure Time 16.0 hour
@Temperature 24.0 °C
Functional cure
 168 hour
@Temperature 24.0 °C
As Tested
Pot Life 45.0 min
@Temperature 23.9 °C
 
Descriptive Properties
Aggregate/Liquid Ratio4:1By volume
 6:1By weight
Chemical/Solvent ResistanceAmmonia: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Chlorinated Solvent: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Hydrochloric Acid 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Kerosene: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Methanol: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Perchloroethylene: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hydroxide 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Sulfuric Acid 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Toluene: poor30 day immersion at 75°F. Sample cured 7 days at RT
ColorLight GreyCured
Coverage4 ft²Cured. @ 1/4"/10 lb. unit
Mix Ratio by volume4.5:1
Mix Ratio by weight5.5:1
Recoat Time6 to 8 hrs
ViscosityPutty-paste. Mixed.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWD9211 / 239720

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.