MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Danquinsa DANCOLL® 255-28 Poly adduct
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DANCOLL® 255-28 is a poly adduct in an organic solvent. It shows very well adhesion properties on a lot of materials. The product has a very high crystallisation rate and is specially suitable for textile laminations and coatings. Because it are achieved high initial values it can be also made stress bondings by means of this product.

Application: DANCOLL® 255-28 is an optimum polyurethane adhesive system for the lamination of different materials with oneself or among themselves. This poylurethane adduct is mainly used for the coating resp. for the lamination of soft PVC, hard PVC, for divers rubber materials, leather, paper, wood, different structured textiles and even for a lot of other materials. For the lamination it is coated one site of the material with this adhesive. The solvents of the coating were exhausted. After the exhausting the applied adhesive film is nonsticky and dry on the surface. At the later lamination the dried adhesive film is heat reactivated at a minimum temperature of 90°C. The further substrate is laminated and pressed in addition. After a short cooling off period of the adhesive composites it are achieved high initial strengthes. For special high chemical resistances and heat resistance DANCOLL® 255-28 can be crosslinked with the isocyanate crosslinker DANCURE® 246-06. We recommend additions of 5-10%. The pot life is 6 hours after the addition of DANCURE® 245-06.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 23 - 30 %DIN 53.189
Brookfield Viscosity 21000 - 31000 cPRVT
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
AspectLight yellowish liquid
Reactivation temperature90°C
SolventMEK (Methyl ethyl ketone)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDANQ033 / 294453

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.