Compound 5780 is a 70 durometer black colored Buna N elastomer. It exhibits good resistance to heat, water, fuels and oils. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 M2 BF 714 B14 B34 EO14 EO34; M2 BG 714 B14 B34 EA14 EF11 EF21 EO14 EO34; M2 BK 714 B14 B34 EF11 EF21 EO14 Information provided by Pressure Seals Inc. |