MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Acetron® Food Grade Blue 50 POM-C Copolymer Acetal, Extruded (ASTM datasheet)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: The data presented in this datasheet is preliminary data and is subject to change as more data is gathered.

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Key Words: POMC, Polyoxymethylene; Polyacetal
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.42 g/ccASTM D792
Water Absorption 0.18 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 0.74 %Immersion; ASTM D570(2)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 83ASTM D785
Hardness, Rockwell R 119ASTM D785
Hardness, Shore D 82ASTM D2240
Tensile Strength 9000 psiASTM D638
Elongation at Break 60 %ASTM D638
Tensile Modulus 430 ksiASTM D638
Flexural Strength 12000 psiASTM D790
Flexural Modulus 435 ksiASTM D790
Compressive Strength 12900 psi10% Def.; ASTM D695
Compressive Modulus 280000 psiASTM D695
Shear Strength 7900 psiASTM D732
Izod Impact, Notched 1.22 ft-lb/inASTM D256 Type A
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square >= 1.00e+13 ohmEOS/ESD S11.11
 
Thermal PropertiesOriginal ValueComments
CTE, linear 94.0 µin/in-°F
@Temperature -40.0 - 149 °C
ASTM E831
Melting Point 338 °FCrystalline, Peak; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 266 °FASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
Estimated Rating
 
Compliance PropertiesOriginal ValueComments
3A-Dairy No
FDA Yes
NSF YesSTD 51 & 61
USDA Yes
USP Class VI No
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Unacceptable
Acids, Weak Limited
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Limited
Conductive / Static Dissipative No
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable
 
Descriptive Properties
ColorBlue
Machinability11-10, 1=Easier to Machine

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

P1SM00ac / 251105

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.