MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Dow SURLYN™ 1605SBR-E Ionomer
Categories: Polymer; Thermoplastic; Ionomer; Ionomer, Film Grade

Material Notes: Product Description: SURLYN™ 1605SBR-E is an ionomer of ethylene acid copolymer. The resin can be processed in conventional blown film, cast film, sheet extrusion and coextrusion equipment designed to process polyethylene and ethylene copolymer type resins. It is also used in extrusion coating and coextrusion coating equipment designed to process polyethylene and ethylene copolymer type resins.
Features: Sodium Ionomer
Characteristics/Benefits: Contains slip, antiblock, and chill roll release additives

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: Antiblock; Chill Roll Release; Slip

Agency Ratings: FDA 21 CFR 177.1330(a)

Form: Pellets

Processing Method: Blown Film; Cast Film; Coextrusion; Extrusion Coating; Sheet Extrusion

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccISO 1183
 0.952 g/ccASTM D792
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Thermal PropertiesOriginal ValueComments
Melting Point 201 °FPeak; ASTM D3418
 201 °FISO 3146
Vicat Softening Point 147 °FASTM D1525
 147 °FISO 306
 
Descriptive Properties
Freezing Point142°FASTM D3418
 142°FISO 3146
Ion TypeSodium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF562 / 311255

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.