MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Versalis Riblene® AB 10 Film Grade Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Riblene AB 10 is a high molecular weight low density polyethylene resin suitable for blown film extrusion. Riblene AB 10 is characterized by a high melt strength leading to a good bubble stability during extrusion. Films manufactured by Riblene AB 10 are easily heat shrinkable and characterized by optimum mechanical properties.

Applications: Riblene AB 10 is recommended for the production of greenhouse film, heavy duty shrink film and industrial bags.

Property values reported for film extruded with BUR 1:3, thickness 70 µm. Actual properties are typical and may vary depending upon operating conditions and additive package.

Information provided by Versalis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ISO 1183
Thickness 70.0 microns2.76 milAs-tested; BUR 1:3
 60.0 - 250 microns2.36 - 9.84 milRecommended
Melt Flow  0.15 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.15 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 0.60 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.60 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 9.00 MPa1310 psiISO 527-3
Film Tensile Strength at Yield, TD 9.00 MPa1310 psiISO 527-3
Film Elongation at Break, MD 400 %400 %ISO 527-3
Film Elongation at Break, TD 600 %600 %ISO 527-3
Coefficient of Friction, Dynamic >= 0.50>= 0.50ISO 8295
Elmendorf Tear Strength, MD 2.90 g/micron73.7 g/milISO 6383-2
Elmendorf Tear Strength, TD 3.60 g/micron91.4 g/milISO 6383-2
Dart Drop Test 380 g0.838 lbF50; ISO 7765-1/A
Film Tensile Strength at Break, MD 27.0 MPa3920 psiISO 527-3
Film Tensile Strength at Break, TD 25.0 MPa3630 psiISO 527-3
1% Secant Modulus, MD 150 MPa21800 psiISO 527-3
1% Secant Modulus, TD 180 MPa26100 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 109 °C228 °FManufacturer method
Vicat Softening Point 91.0 °C
@Load 1.00 kg
196 °F
@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -75.0 °C<= -103 °FASTM D 746
 
Optical PropertiesMetricEnglishComments
Haze 15 %15 %ISO 14782
Gloss 45 %45 %45°; ASTM D 2457
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 220 °C356 - 428 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENF9801 / 265679

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.