MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Osterman & Co Osterlene® MIPS131.4 Medium Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Product Description: MIPS131.4 is a medium impact polystyrene with balanced physical properties. This polymer is utilized in applications such as scale models, toys, housewares, and containers which require consistency from shot to shot. MIPS131.4 is a good for thing walled parts with complex runners and gates; it runs fast and consistently with easy flow. The natural whiteness of MIPS131.4 allows for brightness of colors and reproducibility of color matches. MIPS131.4 is the base carrier of choice for many color concentrate producers.

Availability: North America
Features: Good Flow; Medium Impact Resistance
Uses: Containers; Household Goods; Toys

Information provided by Osterman & Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 13 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3600 psiASTM D638
Elongation at Yield 45 %ASTM D638
Tensile Modulus 360000 psiASTM D638
Flexural Strength 6500 psiASTM D790
Flexural Modulus 340000 psiASTM D790
Izod Impact, Notched 1.40 ft-lb/inASTM D256
Dart Drop, Total Energy 8.33 ft-lbASTM D3029
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 190 °FASTM D648
Vicat Softening Point 198 °FASTM D1525
Flammability, UL94 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

POSTER135 / 267717

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.