MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Akrochem AKROSORBâ„¢ 19251 -72% TAIC Dispersion
Categories: Other Engineering Material

Material Notes: Product Description: Akrosorb 19251 is a dry powdered dispersion of TAIC absorbed on a synthetic calcium silicate, which is used in conjunction with peroxides to improve crosslink performance. This powdered form offers the compounder an easier, more accurate means of handling and weighing liquid products.

Applications: Akrosorb 19251 (72% TAIC) is an effective coagent for peroxide cured polymers especially saturated and partially saturated backbone types like EPDM, CPE, EVA, FKM and HNBR. Being a type two coagent, TAIC has minimal effect on scorch compared to type one c-agents like acrylated and imide functional co-agents (TMPTMA, ZDA, HVA-2, etc.). Utilizing Akrosorb 19251 will provide the following benefits: lower compression set, higher modulus, higher hardness, lower compound viscosity and improved oil, fuel and chemical resistance. A typical loading of Akrosorb 19251 is between 0.70 phr - 4.20 phr (0.5 - 3.0 active TAIC).

Advantages: Polymer bound or encapsulated dispersions are a proven means of upgrading plant safety, efficiency, quality & raw material control. They eliminate any irritating dust, as well as other potential hazards in handling powders in the plant. The physical form is easy to handle and weigh accurately. As a dispersion, better uniformity of the mix at low process temperatures are possible.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/cc
 
Descriptive Properties
Active0.72
Appearancetan to beige powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH142 / 315060

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.