MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials Stat-Rite® M2809 Acrylic Alloy
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Product Description: M2809 is a static dissipative acrylic alloy. It utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. IDP alloys provide consistent static dissipation even when injection molded into components. Features: Permanently static dissipative; Humidity independent; Clean: low out-gassing, low extractable ionics; Durable: can be used for years. Applications: Cleanroom accessories; Swab handles; Totes
Availability: Asia Pacific, Europe, Latin America, North America
Features: Antistatic; Clean/High Purity; Durable; ESD Protection; Humidity Independent; Low (to None) Ion Content; Low to No Outgassing; Rapid Static Decay
Uses: Handles; Medical/Healthcare Applications; Tool/Tote Box
Appearance: Transparent
Forms: Pellets
Processing Method: Injection Molding

Information provided by Lubrizol Advanced Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3800 psiASTM D638
Elongation at Break 30 %ASTM D638
Tensile Modulus 210000 psiASTM D638
Flexural Modulus 210000 psiASTM D790
Izod Impact, Notched 2.60 ft-lb/inASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+10 ohm-cmASTM D257
Surface Resistance 6.00e+9 ohmESD S11.11
Surface Resistivity per Square 1.00e+10 ohm50% RH; ASTM D257
Static Decay <= 0.10 sec1000 V to 10 V, 50% RH
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 167 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 153 °FUnannealed; ASTM D648
 
Descriptive Properties
Ionic Content15 ng/cm2PO4 Anion, Test Method #3010-4
 20 ng/cm2SO4 Anion, Test Method #3010-4
 20 ng/cm2Cl Anion, Test Method #3010-4
 200 ng/cm2Cation Na
 5 ng/cm2NO3 Anion, Test Method #3010-4
Outgassing15 µg/gStyrene, Test Method #3010-3
 180 µg/gToluene, Test Method #3010-3
 250 µg/gTotal Organics, Test Method #3010-3
 40 µg/gMMA, Test Method #3010-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLUBR6014 / 268316

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.