Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 1.70 g/cc | 1.70 g/cc |
Water Absorption | 0.0070 % | 0.0070 % |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore D | 72 | 72 |
Tensile Strength, Ultimate | 47.0 MPa | 6820 psi |
Elongation at Break | 300 % | 300 % |
Flexural Modulus | 1.20 GPa | 174 ksi |
Compressive Strength | 17.0 MPa | 2470 psi |
Izod Impact, Notched | NB | NB |
| NB @Temperature -60.0 °C | NB @Temperature -76.0 °F |
| NB @Temperature 121 °C | NB @Temperature 250 °F |
| NB @Temperature 204 °C | NB @Temperature 399 °F |
Coefficient of Friction | 0.30 - 0.40 | 0.30 - 0.40 |
|
Electrical Properties | Metric | English | Comments |
---|
Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm |
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm |
Dielectric Constant | 2.28 @Frequency 1.36e+10 Hz | 2.28 @Frequency 1.36e+10 Hz |
| 2.31 @Frequency 3.00e+9 Hz | 2.31 @Frequency 3.00e+9 Hz |
| 2.33 @Frequency 1e+9 Hz | 2.33 @Frequency 1e+9 Hz |
| 2.44 @Frequency 1e+8 Hz | 2.44 @Frequency 1e+8 Hz |
| 2.5 - 2.6 @Frequency 1e+6 Hz | 2.5 - 2.6 @Frequency 1e+6 Hz |
| 2.6 @Frequency 1000 Hz | 2.6 @Frequency 1000 Hz |
| 2.6 @Frequency 10000 Hz | 2.6 @Frequency 10000 Hz |
| 2.6 @Frequency 100000 Hz | 2.6 @Frequency 100000 Hz |
Dielectric Strength | 15.0 kV/mm @Thickness 3.20 mm | 381 kV/in @Thickness 0.126 in |
| 70.0 kV/mm @Thickness 0.250 mm | 1780 kV/in @Thickness 0.00984 in |
Dissipation Factor | 0.00070 @Frequency 1000 Hz | 0.00070 @Frequency 1000 Hz |
| 0.0011 @Frequency 10000 Hz | 0.0011 @Frequency 10000 Hz |
| 0.0023 @Frequency 100000 Hz | 0.0023 @Frequency 100000 Hz |
| 0.0072 @Frequency 1e+6 Hz | 0.0072 @Frequency 1e+6 Hz |
| 0.0073 @Frequency 1.36e+10 Hz | 0.0073 @Frequency 1.36e+10 Hz |
| 0.0119 @Frequency 3.00e+9 Hz | 0.0119 @Frequency 3.00e+9 Hz |
| 0.0172 @Frequency 1e+9 Hz | 0.0172 @Frequency 1e+9 Hz |
| 0.023 @Frequency 1e+8 Hz | 0.023 @Frequency 1e+8 Hz |
Arc Resistance | 122 sec | 122 sec |
|
Thermal Properties | Metric | English | Comments |
---|
Heat of Fusion | 43.8 J/g | 18.8 BTU/lb |
CTE, linear | 133 µm/m-°C @Temperature 0.000 - 100 °C | 73.9 µin/in-°F @Temperature 32.0 - 212 °F |
| 209 µm/m-°C @Temperature 100 - 150 °C | 116 µin/in-°F @Temperature 212 - 302 °F |
| 257 µm/m-°C @Temperature 150 - 200 °C | 143 µin/in-°F @Temperature 302 - 392 °F |
Specific Heat Capacity | 1.05 J/g-°C @Temperature 25.0 °C | 0.250 BTU/lb-°F @Temperature 77.0 °F |
| 1.26 J/g-°C @Temperature 100 °C | 0.300 BTU/lb-°F @Temperature 212 °F |
| 1.42 J/g-°C @Temperature 150 °C | 0.340 BTU/lb-°F @Temperature 302 °F |
| 1.59 J/g-°C @Temperature 300 °C | 0.380 BTU/lb-°F @Temperature 572 °F |
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F |
Melting Point | 255 - 280 °C | 491 - 536 °F |
Maximum Service Temperature, Air | 150 °C | 302 °F |
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F |
Deflection Temperature at 1.8 MPa (264 psi) | 51.0 °C | 124 °F |
Flammability, UL94 | V-0 | V-0 |
Oxygen Index | 30 - 32 % | 30 - 32 % |
|
Optical Properties | Metric | English | Comments |
---|
Transmission, Visible | 94 % @Thickness 0.0250 mm, Wavelength 400 nm | 94 % @Thickness 0.000984 in, Wavelength 400 nm |
| 94 % @Thickness 0.0250 mm, Wavelength 500 nm | 94 % @Thickness 0.000984 in, Wavelength 500 nm |
| 94 % @Thickness 0.0250 mm, Wavelength 600 nm | 94 % @Thickness 0.000984 in, Wavelength 600 nm |
| 95 % @Thickness 0.0250 mm, Wavelength 700 nm | 95 % @Thickness 0.000984 in, Wavelength 700 nm |
| 95 % @Thickness 0.0250 mm, Wavelength 800 nm | 95 % @Thickness 0.000984 in, Wavelength 800 nm |
UV Transmittance | 91.5 % @Thickness 0.0250 mm, Wavelength 200 nm | 91.5 % @Thickness 0.000984 in, Wavelength 200 nm |
| 92 % @Thickness 0.0250 mm, Wavelength 250 nm | 92 % @Thickness 0.000984 in, Wavelength 250 nm |
| 92 % @Thickness 0.0250 mm, Wavelength 300 nm | 92 % @Thickness 0.000984 in, Wavelength 300 nm |
| 93 % @Thickness 0.0250 mm, Wavelength 350 nm | 93 % @Thickness 0.000984 in, Wavelength 350 nm |
|
Processing Properties | Metric | English | Comments |
---|
Processing Temperature | 302 - 323 °C | 576 - 613 °F |
|
Descriptive Properties |
---|
20% Hydrochloric Acid Transmission, g/100sq in. | <0.02 |
50% Sodium Hydroxide Transmission, g/100sq in. | <.02 |
Acetic Acid Transmission, g/100sq in. | 0.41 |
Acetone Transmission, g/100sq in. | 0.95 |
Acetophenone Transmission, g/100sq in. | 0.5 |
Benzene Transmission, g/100sq in. | 0.64 |
Carbon Tetrachloride Transmission, g/100sq in. | 0.31 |
Chemical/Solvent Resistance | Excellent |
Ethyl Acetate Transmission, g/100sq in. | 0.76 |
Folding Endurance, # cycles, .18-.20 mm | 10-27 E3 |
Heat of Combustion J/g | 13700 |
Hexane Transmission, g/100sq in. | 0.56 |
Piperidine Transmission, g/100sq in. | 0.04 |
Red Fuming Nitric Acid Transmission, g/100sq in. | 7.5-1.4 |
Salt Spray Resistance on aluminum, Hours | 1000 |
Sulfuric Acid Transmission, g/100sq in. | 0.00001 |
Water Transmission, g/100sq in. | 0.4 |
Weather Resistance | 15 |