MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

SABIC 2501N0W LDPE (Global)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: SABIC® LDPE 2501N0W is a grade without additives with a low gel level, which combines good draw down ability with fair optical properties and stiffness. Application SABIC® LDPE 2501N0W is typically used in diaper film, surface protection film, lamination film and in applications where low blocking behavior is required and the presence of slip and anti block is unwanted. SABIC® LDPE 2501N0W can typically be used for food applications due to very low migration levels. Film properties Film properties have been measured at film of 50 µm with a BUR of 3. The film has been produced on Kiefel IBC blown film line with 200 kg/h. Die size 200 mm, die gap 0.8 mm. This product is not intended for and must not be used in any pharmaceutical/medical applications.

Information provided by Sabic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.925 g/cc0.0334 lb/in³ASTM D1505
Melt Flow 0.75 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.75 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, TD 12.0 MPa1740 psiASTM D882
Film Elongation at Break, MD >= 200 %>= 200 %ASTM D882
Film Elongation at Break, TD >= 500 %>= 500 %ASTM D882
Tensile Modulus 0.200 GPa29.0 ksiTD; ASTM D882
Coefficient of Friction 0.900.90ASTM D1894
Tear Strength 45.0 kN/m257 pliTD; ISO 6383-2
 45.0 kN/m257 pliMD; ISO 6383-2
Dart Drop Total Energy 150 J/cm0.281 ft-lb/milASTM D4272
Film Tensile Strength at Break, MD 25.0 MPa3630 psiASTM D882
Film Tensile Strength at Break, TD 20.0 MPa2900 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 98.0 °C208 °Fat 10 N (VST/A); ISO 306
 
Optical PropertiesMetricEnglishComments
Haze 10 %10 %ASTM D1003
 
Descriptive Properties
Blocking20 gSABIC method
Clarity25 mVSABIC method
Re-blocking<5 gSABIC method

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI30334 / 228724

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.