MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Plenco 6404 Two-Stage Phenolic, Transfer Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Mineral/Glass Filled

Material Notes: PLENCO 06404 is a black glass fiber and mineral filled two-stage phenolic molding compound offering superior molded mechanical properties, especially tensile strength. PLENCO 06404 is UL recognized under component file E40654.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.660 g/ccASTM D1895
Density 1.72 g/ccASTM D792
Water Absorption 0.080 %ASTM D570
Linear Mold Shrinkage 0.0012 cm/cmASTM D6289
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell E 100ASTM D785
Tensile Strength, Ultimate 148 MPaASTM D638
Elongation at Break 1.1 %ASTM D638
Tensile Modulus 16.8 GPaASTM D638
Flexural Strength 219 MPaASTM D790
Flexural Modulus 17.0 GPaASTM D790
Compressive Strength 300 MPaASTM D695
Izod Impact, Notched 55.8 J/mASTM D256
Impact 386J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.20e+11 ohm-cmASTM D247
Dielectric Constant 5.3
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 13.2 kV/mmshort time; ASTM D149
Dissipation Factor 0.039
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 120 secASTM D495
Comparative Tracking Index 185 VASTM D3638
 
Thermal PropertiesOriginal ValueComments
CTE, linear 38.0 µm/m-°CASTM E831
Maximum Service Temperature, Air 240 °CHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 270 °CASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
ASTM D150
 5VA
@Thickness 1.50 mm
ASTM D150
Shrinkage 0.030 %Post Shrinkage 72 hr, 120ºC; ASTM D6289
 
Descriptive Properties
FormBriquette

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLEM11q / 243104

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.