MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
American Elements Ytterbium Nanoparticles
Categories: Metal; Nonferrous Metal; Pure Element

Material Notes: General Description

Ytterbium (Yb) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Ytterbium Particles are typically 10 - 80 nanometers (nm) with specific surface area (SSA) in the 30 – 60 m 2 /g range. Nano Ytterbium Particles are also available in passivated and Ultra high purity and high purity and coated and dispersed forms. Research into applications for Ytterbium nanocrystals has focused on use for high-power fiber lasers and amplifiers, as a dopant or by direct deposition in glass, laser optics and optical fibers, in phosphors, nanophosphors and doped phosphorous nanoparticles and for their potential magnetic, optical, imaging, biomedical and bioscience properties and for use in coatings, plastics, nanowire, and in alloy and catalyst applications.

Key Words: Formula: Yb; CAS Number: 7440-64-4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.57 g/cc
Particle Size 0.010 - 0.080 µm
Specific Surface Area 30 - 60 m²/g
Molecular Weight 173.04 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point 824 °C
Boiling Point 1196 °C
 
Descriptive Properties
AppearanceBlack
StabilityEasily oxidized in air

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Gold, Au
Overview of materials for 7000 Series Aluminum Alloy
Tantalum, Ta; Cold Worked
Overview of materials for 5000 Series Aluminum Alloy
Overview of materials for 4000 Series Aluminum Alloy

EJAMER94 / 5577

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.