23% Carbon-Fiber-Filled Nylon 12 optimized for stiffness and sustainable accuracy at elevated temperatures. Highlights: - High-Detail Surface Finish
- Fine-Feature Resolution
- Dimensional Stability at Elevated Temperatures
Applications: - Under hood engine components
- Rapid tooling applications
- Wind tunnel model testing
Information provided by Advanced Laser Materials |