MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Osterman & Co Osterlene® HM0550 High Density (HMW) Polystyrene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: Product Description: HM0550 is a high molecular weight high density polyethylene (HMW-HDPE) for film extrusion and extruded sheet/thermoforming applications. It is a bi-modal resin designed for high impact strength and good processing characteristics. This resin is well balanced in overall physical properties and provides good stiffness for thin gauge film and extruded sheet/thermoforming applications. Suggested applications for HM0550 include heavy duty bags, industrial liners, t-shirt bags and trash can liners.

Availability: North America
Features: Good Processability; Good Stiffness; High Impact Resistance; High Molecular Weight
Uses: Film; Heavy-duty Bags; Industrial Applications; Liners
Processing Method: Extrusion; Film Extrusion; Sheet Extrusion; Thermoforming

Information provided by Osterman & Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.949 g/ccASTM D792
Melt Flow 0.040 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 8.5 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 300 %ASTM D882
Film Elongation at Break, TD 410 %ASTM D882
Elmendorf Tear Strength MD 14 gASTM D1922
Elmendorf Tear Strength TD 25 gASTM D1922
Dart Drop Test 210 gF50; ASTM D1709
Film Tensile Strength at Break, MD 9000 psiASTM D882
Film Tensile Strength at Break, TD 4100 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 268 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

POSTER050 / 267632

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.