MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Master Bond Supreme 11AOHTMed Two Component Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: Key Features:
  • Convenient handling
  • Thermally conductive & electrically insulative
  • Exceptionally high physical strength profile
  • Meets ISO 10993-5
Product Description: Master Bond Supreme 11AOHTMed is a two part, room temperature curing epoxy for bonding and sealing. It is a faster curing system with a paste consistency and a forgiving 1 to 1 mix ratio by weight. It is formulated to cure readily at ambient temperatures or more rapidly at elevated temperatures. The optimum curing schedule is overnight at room temperature followed by 2-3 hours at 120°F to 150°F. The epoxy is 100% reactive and contains no solvents or diluents. It has low shrinkage and high dimensional stability. The system bonds well to a wide variety of substrates including most metals, ceramics, and glass as well as many rubbers and plastics. Supreme 11AOHTMed is well suited for bonding dissimilar substrates. and is a toughened system that withstands rigorous thermal cycling. While it is thermally conductive, it is still a dependable electrical insulator. Supreme 11AOHTMed is resistant to many sterilants including EtO, gamma, radiation, glutaraldehyde and hydrogen peroxide, among others. The color of Part A is gray and the color of Part B is off-white. Supreme 11AOHTMed is a good candidate for applications where high strength bonding in medical device manufacturing is critical. Its thermal conductivity also can be desirable in certain situations. However, what makes this system so special is its super high strength profile.

Product Advantages:

  • One to one mix ratio, fast setting
  • Versatile cure schedules
  • High physical strength properties, especially lap shear
  • Can withstand rigorous thermal cycling
  • Passes ISO 10993-5

Information provided by Master Bond, Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 200000 - 300000 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80.0 - 90.0
 85.0
@Treatment Temp. 85.0 °C,
Time 3.60e+6 sec
aging at 85% RH
Tensile Strength 7000 - 80000 psi
Tensile Modulus 400000 - 450000 psi
Compressive Strength 20000 - 22000 psi
Adhesive Bond Strength 3200 - 3400 psilap shear, aluminum to aluminum
Peel Strength 15.0 - 20.0 pliT-peel, aluminum to aluminum
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 4.60
 
Thermal PropertiesOriginal ValueComments
CTE, linear 35.0 - 40.0 µm/m-°C
Thermal Conductivity 0.580 - 0.720 W/m-K
Maximum Service Temperature, Air 204 °C
Minimum Service Temperature, Air -80.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 - 2.00 hour
@Temperature 93.3 °C
option
 24.0 - 46.0 hour
@Temperature 23.9 °C
option
Working Life 15.0 - 25.0 minafter mixing, 100 gram batch
Shelf Life 6.00 Monthin original, unopened containers
 
Descriptive Properties
Mixing ratio1:1Part A to B
Optimum cure scheduleovernight at 75°F followed by 2-3 hours at 120-150°F
ViscosityThixotropic pastePart B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMASTM5810 / 323327

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.