MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

RAMPF RAKU® TOOL InnoTuf® TP-4070 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: High Impact / High Heat; Rigid polyurethane

Key Properties:

  • Excellent physical properties after post cure
  • Low viscosity
  • Free of mercury, MOCA, TDI, PBDE, or phthalates
  • Excellent impact resistance
  • RoHS & REACH compliant
Applications:
  • For hand-batch or meter mix processing
  • For short run and prototype parts
Cure 1: 16 hours at 180°F

Information provided by © RAMPF Tooling Solutions GmbH & Co. KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³Hardener; ASTM D-792
 1.13 g/cc0.0408 lb/in³Cure 1; ASTM D-792
 1.16 g/cc0.0419 lb/in³Resin; ASTM D-792
Viscosity 400 cP400 cPResin; ASTM D-2393
 600 cP600 cPMix; ASTM D-2393
 900 cP900 cPHardener; ASTM D-2393
Linear Mold Shrinkage 0.0010 - 0.0050 cm/cm0.0010 - 0.0050 in/inCure 1; ASTM D-2566
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 75 - 8575 - 85Cure 1; ASTM D-2240
Tensile Strength 69.947 MPa10145 psiCure 1; ASTM D-638
Elongation at Break 26 %26 %Cure 1; ASTM D-638
Flexural Strength 105 MPa15200 psiCure 1; ASTM D-790
Flexural Modulus 2.58028 GPa374.238 ksiCure 1; ASTM D-790
Izod Impact, Notched 1.12 J/cm2.10 ft-lb/inCure 1; ASTM D-256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C185 °FCure 1; ASTM D-648
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 - 180 min1.00 - 3.00 hourMix, Demold time
Gel Time 5.00 - 8.00 min5.00 - 8.00 minMix
 
Descriptive Properties
AspectWhiteCure 1
Mix Ratio100:47Resin: Hardener, Weight
 100:50Resin: Hardener, Volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRAMPF041 / 317641

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.