Product Description: Modified PPE; PA/PPE alloy; Flame Retardant V-0; Easy Flow Availability: Africa & Middle East; Asia Pacific; Europe; North America Additive: Flame Retardant; Halogen Free; High Flow Processing Method: Injection Molding Part Marking Code (ISO 11469): PP66+PPE-FR(51) Information provided by Asahi Kasei Corporation |