MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

SABIC ULTEM™ Resin HU2310 Polyetherimide (PEI) (Europe)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI); food contact compliant; Steam, Gamma, EtO, and E-beam sterilizable.

Features: Healthcare,High Stiffness,Steam, Gamma, EtO and E-beam sterilizable,Hydrolytic Stability,Chemical Resistance,Low Smoke and Toxicity,Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,Low Shrinkage,Good metal adhesion,Amorphous,High Strength,High Heat Resistance,Good dimensional stability,Flame Retardant,Steam Sterilizable,Gamma Sterilizable,E-beam Sterilizable,Food Contact Acceptable,Biocompatible

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.51 g/cc1.51 g/ccASTM D792
Density 1.51 g/cc0.0546 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.500 %0.500 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.90 %0.90 %ISO 62-1
Viscosity 8.0 cP
@Load 5.00 kg,
Temperature 360 °C
8.0 cP
@Load 11.0 lb,
Temperature 680 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0040 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 7.6 g/10 min
@Load 6.60 kg,
Temperature 337 °C
7.6 g/10 min
@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 158 MPa22900 psi5 mm/min; ASTM D638
 165 MPa23900 psi5 mm/min; ISO 527
Tensile Strength, Yield 165 MPa23900 psi5 mm/min; ISO 527
 168 MPa24400 psi5 mm/min; ASTM D638
Elongation at Break 2.0 %2.0 %5 mm/min; ISO 527
 3.0 %3.0 %5 mm/min; ASTM D638
Elongation at Yield 2.0 %2.0 %5 mm/min; ISO 527
 3.0 %3.0 %5 mm/min; ASTM D638
Tensile Modulus 9.23 GPa1340 ksi5 mm/min; ASTM D638
 9.50 GPa1380 ksi1 mm/min; ISO 527
Flexural Strength 220 MPa31900 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 225 MPa32600 psiyield, 2 mm/min; ISO 178
Flexural Modulus 8.50 GPa1230 ksi2 mm/min; ISO 178
 9.25 GPa1340 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 85.0 J62.7 ft-lbASTM D256
 90.0 J
@Temperature -30.0 °C
66.4 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 10.0 J7.38 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 60 - 120 sec60 - 120 secASTM D495
Comparative Tracking Index 100 - 175 V100 - 175 VUL 746A
Hot Wire Ignition, HWI  15 - 30 sec
@Thickness >=1.50 mm
15 - 30 sec
@Thickness >=0.0591 in
UL 746A
 60 - 120 sec
@Thickness >=3.00 mm
60 - 120 sec
@Thickness >=0.118 in
UL 746A
High Amp Arc Ignition, HAI  0.00 - 15 arcs
@Thickness >=3.00 mm
0.00 - 15 arcs
@Thickness >=0.118 in
UL 746A
 15 - 30 arcs
@Thickness >=1.50 mm
15 - 30 arcs
@Thickness >=0.0591 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min3.15 - 5.91 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  16.0 µm/m-°C
@Temperature -20.0 - 150 °C
8.89 µin/in-°F
@Temperature -4.00 - 302 °F
ASTM E831
 16.0 µm/m-°C
@Temperature 23.0 - 150 °C
8.89 µin/in-°F
@Temperature 73.4 - 302 °F
ISO 11359-2
CTE, linear, Transverse to Flow  41.0 µm/m-°C
@Temperature -20.0 - 150 °C
22.8 µin/in-°F
@Temperature -4.00 - 302 °F
ASTM E831
 41.0 µm/m-°C
@Temperature 23.0 - 150 °C
22.8 µin/in-°F
@Temperature 73.4 - 302 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 208 °C
@Thickness 3.20 mm
406 °F
@Thickness 0.126 in
unannealed; ASTM D648
 210 °C
@Thickness 6.40 mm
410 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 213 °C415 °FRate B/50; ISO 306
 220 °C428 °FRate B/120; ISO 306
 228 °C442 °FRate B/50; ASTM D1525
UL RTI, Electrical 180 °C356 °FUL 746B
UL RTI, Mechanical with Impact 170 °C338 °FUL 746B
UL RTI, Mechanical without Impact 180 °C356 °FUL 746B
Flammability, UL94  V-0
@Thickness >=0.250 mm
V-0
@Thickness >=0.00984 in
UL 94
 5VA
@Thickness >=1.20 mm
5VA
@Thickness >=0.0472 in
UL 94
Glow Wire Ignition Temperature 900 °C
@Thickness 2.00 mm
1650 °F
@Thickness 0.0787 in
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 345 - 400 °C653 - 752 °F
Zone 2 340 - 400 °C644 - 752 °F
Zone 3 345 - 400 °C653 - 752 °F
Melt Temperature 350 - 400 °C662 - 752 °FInjection Molding
Mold Temperature 135 - 165 °C275 - 329 °F
Drying Temperature 150 °C302 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
 24.0 hour24.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82731 / 290678

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.