NAV101 is a transparent low density polyethylene post-consumer recycled (rLDPE) supplied in pellet form for high-end blown film applications. NAV101 is an ideal LDPE used where sustainability and circularity matter. NAV101 is a 100% post-consumer recycled including a large part of recycled post-consumer plastic waste coming from pre-sorted municipal (household) waste. NAV101 is part of the EuCertPlast certificate according to the European Standard EN 15343:2007 (certificate available upon request). Due to the nature of recycleds, some variation in color can be observed between batches. Cas No. 9002-88-4 Typical characteristics: - High transparency
- Available in homogenized 24-ton truckloads
- Low odor
- Filtration: 100 µm
Applications:- Collation shrink film
- Shrink film
- Lamination film for non-food contact primary packaging
- Non-food contact primary packaging
- Secondary and tertiary packaging where transparency is key
Note: Minor quantity of BorShape" LLDPE significantly boosts mechanical performance, brand owners and retailers meeting their sustainability goals without compromising key mechanical properties for similar packaging performanceInformation provided by Borealis AG |