MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lubrizol ESTANE® ALR CL90A-VE EXP Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Type: Aliphatic polycaprolactone based Thermoplastic Polyurethane (TPU) with a 90 Shore A Hardness.

Features: Clear resin with excellent colour stability upon weather exposure. This high performance resin is UV resistant and has excellent mechanical properties. This product provides high quality film and excellent transparency.

Uses: Blown and Cast film extrusion, outdoor applications, protective films and graphic films.

Information provided by The 159 Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/ccISO 2781
Maximum Moisture Content 0.020
Melt Flow 10 - 20 g/10 min
@Load 10.0 kg,
Temperature 170 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90
@Time 3.00 sec
ISO 868
Tensile Strength 45.0 MPaISO 527
Elongation at Break 550 %ISO 527
100% Modulus 7.00 MPa
@Strain 100 %
ISO 527
300% Modulus 20.0 MPa
@Strain 300 %
ISO 527
 
Processing PropertiesOriginal ValueComments
Zone 1 165 - 175 °CExtrusion
 170 - 180 °CBlown Film
Zone 2 175 - 185 °CExtrusion
 180 - 190 °CBlown Film
Zone 3 175 - 185 °CExtrusion
 190 - 200 °CBlown Film
Zone 4 185 - 195 °CExtrusion
Adapter Temperature 185 - 195 °CExtrusion, (5)
 195 - 205 °CBlown Film, Zone 4
Die Temperature 190 - 200 °CExtrusion, Die Zone 1 (6)
 190 - 200 °CExtrusion, Die Zone 2
 195 - 205 °CBlown Film, Zone 5 (Die Z. Upper)
 195 - 205 °CBlown Film, Zone 6 (Die Z. Lower)
Drying Temperature 60.0 °C
@Time 14400 sec
Moisture Content <= 0.10 %MQSA 44
Dew Point -40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Estane® ALR CL65D Thermoplastic Polyurethane
Lubrizol Estane® ALR PC95A Thermoplastic Polyurethane
Lubrizol Estane® ALR E87A Thermoplastic Polyurethane
Lubrizol Advanced Materials Pearlthane® ECO D12T85 Thermoplastic Polyurethane
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer

PLUBR5000 / 238870

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.